Lokacin zabar kayan rufin da suka dace, ana fifita zanen gado na galvanized saboda dorewarsu da sauƙin amfani. Jindalai Steel Group Co., Ltd. tana ba da zaɓuɓɓuka iri-iri, gami da zanen gado na galvanized mai electro-galvanized, zanen gado na galvanized mai zafi, zanen gado na zinc mai aluminum, zanen gado na galvanized aluminum-magnesium mai galvanized, da zanen gado na galvanized mai launi. Kowane nau'in zanen gado yana da nasa halaye na musamman, wanda hakan ke sa ya zama mahimmanci a fahimci bambance-bambancen su da aikace-aikacen su.
Babban bambanci tsakanin zanen gado mai laushi na galvanized mai zafi da zanen gado mai laushi na electro-galvanized
Babban bambanci tsakanin zanen gado mai laushi da aka yi da galvanized mai zafi da kuma na lantarki yana cikin tsarin shafa su. Galvanizing mai zafi ya ƙunshi nutsar da zanen ƙarfe a cikin zinc mai narkewa, wanda ke haifar da kauri da ƙarfi tare da juriyar tsatsa. Wannan hanyar ta dace da amfani a cikin mawuyacin yanayi, kamar yankunan bakin teku ko wuraren danshi mai yawa, inda danshi da gishiri ke hanzarta tsatsa.
A gefe guda kuma, ana samar da takardar corrugated mai amfani da lantarki ta hanyar shafa wani Layer na zinc a saman takardar ta hanyar amfani da lantarki. Wannan tsari yana samar da siraran zinc, wanda hakan ya sa ya dace da aikace-aikacen cikin gida ko muhallin da ke da ƙarancin lalata. Duk da cewa takardar electro-galvanized ba ta da tsada sosai, aikin kariyarta na iya zama ba daidai da takardar galvanized mai zafi ba.
Yaya;Don Zaɓar Takardar Corrugated Mai Daidai Don Muhalli na Teku/Mai Yawan Danshi
Ga yanayin bakin teku ko kuma yanayin zafi mai yawa, ana ba da shawarar zanen gado mai kauri da aka yi da galvanized mai zafi. Layin zinc ɗinsu mai kauri yana hana tsatsa da tsatsa yadda ya kamata, yana tabbatar da tsawon rai da dorewa. A madadin haka, ana iya la'akari da zanen gado mai kauri da aka yi da galvanized aluminum-magnesium alloy, domin suna ba da kyakkyawan juriya ga tsatsa yayin da suke riƙe da ƙira mai sauƙi.
Tabbatar da Mannewar Rufin Zinc
Domin tantance mannewar murfin zinc da sauri akan zanen gado mai kauri, ana iya yin gwaji mai sauƙi. "Gwajin gogewa" ya ƙunshi amfani da ruwan wuka mai kaifi don ƙirƙirar tsarin grid a saman murfin. Bayan shafa tef a kan grid, cire shi yana ba ku damar lura da mannewar da ke tsakanin layin zinc da substrate. Idan layin zinc ya kasance ba shi da matsala, mannewar yana da kyau; in ba haka ba, yana iya nuna matsalar inganci.
Hana tsatsa fari daga samuwa yayin ajiya
Tsatsa fari matsala ce da ake yawan samu a kan zanen ƙarfe mai kauri, wanda yawanci ke faruwa ne sakamakon taruwar danshi yayin ajiya. Don hana tsatsa fari, dole ne a adana zanen da aka yi da kauri mai kauri a wuri busasshe, mai iska mai kyau. Amfani da kayan da ke sha danshi, kamar su silica gel desiccants, na iya taimakawa wajen rage danshi. Bugu da ƙari, guje wa cunkoson zanen yana haɓaka zagayawar iska kuma yana rage haɗarin samuwar farin tsatsa.
Kauri na Rufin da Aka Yi Amfani da Shi da Tsayin Raƙuman Ruwa
Ana samun zanen gado mai kauri iri-iri da tsayin raƙuman ruwa don biyan buƙatun rufin daban-daban. Kauri na yau da kullun yana tsakanin 0.3 mm zuwa 1.2 mm, kuma tsayin raƙuman ruwa yawanci yana tsakanin 18 mm zuwa 76 mm. Zaɓin kauri da tsayin raƙuman ruwa ya dogara da dalilai da yawa, kamar amfanin da aka yi niyya, buƙatun ɗaukar kaya, da fifikon kyau.
A takaice dai, zabar takardar da ta dace ta corrugated mai galvanized yana da matuƙar muhimmanci wajen tabbatar da dorewa da kuma aikin ayyukan rufin. Jindalai Steel Group Co., Ltd. ta himmatu wajen samar da kayayyaki na musamman masu inganci don biyan buƙatunku na musamman. Ko kun zaɓi galvanizing mai zafi, electro-galvanizing, ko wani nau'in, ƙungiyar ƙwararrunmu za ta yi farin cikin shiryar da ku da kuma taimaka muku yin zaɓi mafi kyau don buƙatun aikace-aikacenku.
Lokacin Saƙo: Fabrairu-09-2026